1.Scope

This standard specifies the product classification, technical requirements, test methods, acceptance rules, packaging and labeling requirements, transportation and storage of polypropylene spunbond / meltblown / spunbond composite non woven fabric ( hereinafter referred to as SMS ).

This standard applies to 10 g / m2 — > 80g / m2 polypropylene SMS products with polypropylene as the main raw material

2.Normative references

The clauses in the following documents become the clauses of this standard through quotation from this standard. For dated reference documents, all subsequent amendments ( not including errata content ) or revisions are not applicable to this standard. However, parties that have reached an agreement based on this standard are encouraged to study whether the latest versions of these documents. For the cited documents without date, the latest version is applicable to this standard.

spunbond nonwoven

GB / T 4744 Determination of water permeability resistance of textile fabrics, hydrostatic pressure test

GB / T 5453 Textiles, fabric breathability determination

GB / T 6529 Standard atmosphere for humidity control and testing of textiles

FZ / T 60003 Determination of mass per unit area of nonwoven fabric

FZ / T 64004 Thin - bonded nonwoven fabric

FZ / T 60005 Determination of breaking strength and breaking elongation of non woven fabric roll

3.Terms

GB / T3291.3 established and the following terms apply to this standard

3.1 Hard block

Refers to the hard lumps caused by the dripping of the melt.

3.2 stiff wire

Refers to the unstretched hard wire.

3.3 Turning the Net

It refers to the phenomenon that the fiber web is seriously uneven due to being hung by foreign objects before being reinforced.

3.4 folding

It refers to the superposition of fiber webs that are superimposed together and after reinforcement, different from other places.

3.5 Hole

Holes with an area of more than 4mm2, with no fiber in the middle are holes.

4.Technical requirements

4.1 Polypropylene chips ( whether raw materials are required )

4.2 Physical properties

The physical properties of the product should meet the requirements of Table

Quality 0 291.3 Table 1 Physical performance requirement

Mass per unit area

g / m2

11-13

> 13-17

> 17-21

> 21-25

> 25-30

> 30-35

> 35-40

> 40-50

> 50-60

> 60-70

> 70-80

> 80

Mass deviation rate per unit area:

%

≤ ± 6%,

≤ ± 4%,

Single value deviation per unit area

%

≤ ± 12%

Longitudinal breaking strength

N / 5cm

> 18

> 23


Nous contacter

Author:

Mr. Hua Mao

Phone/WhatsApp:

+8618665305664

Produits populaires
You may also like
Related Categories

Envoyer à ce fournisseur

Sujet:
Portable:
E-mail :
message:

Your message must be betwwen 20-8000 characters

Accueil

Product

Phone

À propos de nous

Demande

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

envoyer